Item : 019409
Name : Alloys - Low Melting Point
Price : Contact us
Details:
Property Indalloy
117 158 160-190 217-440 255 281
Melting Point or Range Deg/F 117 158 160-190 217-440 255 281
Weight lbs/in3 .32 .339 .341 .343 .380 .315
Tensile Strength lbs/in2 5,400 5,990 5,400 13,000 6,400 8,000
Brinell Hardness No. 12 9.2 9 .19 10.2 22
Maximum Load
30 sec lbs/in2 --- 10,000 9,000 16,000 8,000 15,000
Safe Load Sustained --- 300 300 300 300 500
Conductivity (Electrical)
Compared with Pure Copper 3.34% 4.17% 4.27% 2.57% 1.75% 5.00%
Cumulative Growth and Shrinkage Time after Casting
2 min. +.0005 +.0025 -.0004 +.0008 -.0008 +.0007
6 min. +.0002 +.0027 -.0007 +.0014 -.0011 +.0007
30 min. .0000 +.0045 -.0009 +.0047 -.0010 +.0006
1 hr. -.0001 +.0051 .0000 +.0048 -.0008 +.0006
2 hr. -.0002 +.0051 +.0016 +.0048 -.0004 +.0006
5 hr. -.0002 +.0051 +.0018 +.0049 .0000 +.0005
500 hr. -.0002 +.0057 +.0025 +.0061 +.0022 +.0005